Table of Contents

Put the inspection sections on the finished bend drawing and give each a reference the supplier and buyer can reproduce. Specify how the order defines ovality, where to look for minimum wall and which measurements must appear in the report. The end dimensions of a bent tube leave the condition at the bend unresolved.

Define the geometry at the section being checked

Identify the bend, its orientation and the sections for verification. The buyer might assign positions along the curve and at the transitions, depending on the design. Use the drawing to state which planes or directions are measured. If ovality is defined from maximum and minimum outside diameters, state how the reported difference or percentage is calculated. A percentage needs an explicit reference diameter.

State the wall requirement as a separate characteristic. Identify the specified regions of the section and how the measurement plan addresses the lowest wall reading. A report can include readings on the outside and inside of the curve if the approved plan calls for them. Record actual positions instead of treating one wall reading as proof of the whole bend.

A heat exchanger bundle with U-shaped tubes visible at one end.
U-shaped tubes in a heat exchanger bundle. Specify the inspection sections and reporting basis on the drawing for the bend being purchased.

Ask for a report that can be traced to the part

Report fieldWhat to define in the order
Part and sourceBend or piece ID, drawing revision, forming lot and link to source material where required
Section and orientationLocation along the bend, measurement plane and circumferential reference
OvalityOutside diameters or specified scan result, definition, reference diameter and units
WallReadings and locations, agreed method and limitations, and the minimum reported in the specified region
Acceptance and frequencyApplicable requirements by region, when to inspect, and who approves exceptions

Agree whether the first piece, production pieces or representative samples need measurement. Match the method to the access, surface and precision the requirement needs. If a method cannot examine a region, record that limitation and obtain agreement on the evidence that will be used there.

Keep material conformity and formed geometry traceable

Where specified, ASTM B338 covers seamless and welded titanium and titanium-alloy tubing for condenser and heat exchanger service. Identify the contracted material specification and edition and retain the applicable records. State the formed geometry, inspection method and acceptance requirements for the delivered bend on the drawing or purchase documents. ASTM B338 public scope

Review any difference against the named locations and requirements. The system design authority owns the decision about service, and the supplier records the delivered geometry within the agreed inspection scope.

Frequently asked questions

Can a single reading at the end establish ovality at the bend?

Use measurements from the locations named in the finished bend inspection plan. End readings apply to their own sections.

What is needed when ovality is reported as a percentage?

State the diameter measurements or derived values, the reference diameter, location and exact calculation basis agreed for the order.

Does an ovality result also verify wall thickness?

Require the wall evidence separately at the approved locations. The report should connect both measurements to the same identified bend.

Where should the supplier record the minimum wall?

Identify the section and circumferential location, along with the approved measurement method and the region it covers.

Can the raw tube certificate release the bent part?

Use the certificate for its identified material and tests. Review the required formed-geometry records and approvals for the finished bend.

Who approves an exception to the specified bend geometry?

Use the authorized disposition in the project or purchase documents. Identify the affected bend and the evidence used to make the decision.

Request a formed tube scope review

Send HELE TITANIUM the formed drawing, tubing specification, measurement locations, acceptance requirements and inspection records to be supplied. View titanium tubing · Submit the bend drawing

Prepare a technical enquiry

Share the product form, grade or standard, dimensions, quantity and inspection requirements.

Ask a technical question →

References

Portrait of Bobby Fu

Project contact

Bobby Fu

Co-Founder · Senior Project Manager

Bobby Fu is a co-founder and senior project manager at HELE Titanium, with a background in international product development and manufacturing. His project work covers titanium materials, titanium anodes, and PEM water electrolysis systems. He works with industrial buyers and production teams to clarify material specifications, equipment interfaces, and inspection requirements before orders are placed.

View Bobby’s Profile
WhatsApp